Over the last two years, Industrial Minerals has reported on the shifting trends in the refractories industry with China looking to reduce wastage and increase energy efficiency. This article explores these various trends and asks the important question, "How will this shift impact raw material supply?"
Origin
Uk Consultant
Journal Title
Industrial Minerals Sept/2015 30-32, 34, 36
Sector
Refractories
Class
R 832