Influence of Co60 y-irradiation on the optical properties of vitreous As2S3-GeS2 is studied. The long wave shift of the fundamental optical absorption edge is observed after radiation treatment with 2.2 MGy exposed dose. The initial position of this edge restores to some residual value during the 2-3 months after y-irradiation.