The relation betwen preparation conditions and Tb3+ quantum yield was investigated on silica-based sol-gel glass powders and it was found that the quantum yield depends mainly on the firing temperature.
Origin
Philips Research Laboratories, Eindhoven
Journal Title
Phys Chem Glasses 1989 30 4 162-163
Sector
Special Glass
Class
S 298