The quality control of various types of colemanite used by Vertex at Litomysl is described with particular reference to comparisons between tharmally treated colemanite and synthetic calcium borate.
Origin
Sklo Union, Vertex Litomysl
Journal Title
Sklar A Keramik 1987 37 12 346-348
Sector
Glass Fibre
Class
GF 12