Chemical durability, glass formation tendency, and other properties of iron alumina phosphate glasses containing 70wt% of a simulated high level nuclear waste (HLW), doped with different amounts of Cr203, have been investigated.
Origin
Tongji University, Shanghai, China
Journal Title
Glas Sci Technol 77 5 2004 203-210
Sector
Special Glass
Class
S 2876