The problem involved in developing a technology for the manufacture of continuously rolled white slag ceramics are discussed briefly. The physicochemical properties of the material and possible areas of application have been determined.
Origin
Unknown
Journal Title
Glass And Ceramics 1975 32 (1-2) 11-13
Sector
Primary Papers
Class
PP 299