Compositions and principles of preperation of glass-forming colloidal solutions resistant to gel formation and based on tetraethoxysilane are given. The processes occurring in heating the products of thermal deposition of thr solutions are considered. Using a mathematical experiment design, the effect of molybdenum, manganese, and copper oxides on the strength of adhesion of the coating to the substrate is determined. The moulding conditions and the properties of protective vitreous coatings are indicated.