A method for the production of large-diameter borosilicate tubing by vertical drawing from an electric furnace with a drawing chamber is described.
Origin
State Scientific-Research Institute Of Glass, Gomel Glass Plant
Journal Title
Glass And Ceramics 1987 44 5-6 233-236
Sector
Special Glass
Class
S 120