The procedure is divided into three stages: (1) decomposition of the sample, (2) separation of phosphoric acid from amphoteric and alkaline earth elements, and (3) separation of the alkaline elements from phosphoric acid.
Origin
Unknown
Journal Title
Steklo Inform Mater Inst Stekla 3 1964 72-73
Sector
Primary Papers
Class
PP 1345