Advantages of pressure slip casting over traditional shaping techniques make its use desirable for the manufacture of technical ceramics.
Origin
Centro Ceramico, Italy
Journal Title
Am Ceram Soc Bull 79 11 2000 49-53
Sector
Glass Ceramics
Class
GC 401