It will be reported on the different primary and secondary measures which are employed in recent years in the German Glass Industry to reduce the NOx emissions of glass melting furnaces. The utilization of these different measures led in many cases to a significant reduction of the NOx emission. The results which were reached so far will be reported and discussed.