Oxysulphide glasses were prepared in a wide range of compositions in the system LiBO2-LiBS2. Temperatures of glass transition, crystallisation and liquidus were determined. An electrical conductivity enhancement with the mixing of two components was accompanied by a decrease in the degree of undercooling of the glass.
Origin
University Of Osaka Prefecture
Journal Title
J Am Ceram Soc 1988 71 9 766-769
Sector
Special Glass
Class
S 172