The possibilities of using photosensitive glasses for the miniaturization of electronic components are described with particular reference to the forming of parts on photosensitive glass plates in the Polish Glass and Ceramics Institute.
Origin
Unknown
Journal Title
Szklo I Keramika 1972 23 (2) 40-41
Sector
Primary Papers
Class
PP 719