A better understanding of the microscale mechanisms of polymer-plasticized extrudate flow is required to develop ceramic extrusion technology. Experimental methods for quantifying plastic properties of extrudates under conditions of shear and extensional flow are needed.
Origin
Nysc, Alfred, Usa
Journal Title
Am Ceram Soc Bull 80 6 2001 73-76
Sector
Glass Fibre
Class
GF 283