The system KF-A1F3 was re-investigated precisely by differential thermal analysis, X-ray diffractometry, and visual observation. All of the samples were prepared by solution synthesis.
Origin
Peking University, Beijing, China
Journal Title
J Am Ceram Soc 83 12 2000 3196-3198
Sector
Special Glass
Class
S 2090