The phase diagram of the Ba0(BaCO3)-Ca0-Cu0 system, especially in the barium-rich region at 900 deg C in air, was studied.
Origin
Kurashiki University Of Science And The Arts, Japan
Journal Title
J Am Ceram Soc 82 5 1999 1329-1332
Sector
Special Glass
Class
S 1664