Nine machinable ceramics have been characterised for phase constitution by X-ray diffraction and for microstructure by scanning electron microscopy.
Origin
Hiroshima University School Of Dentistry, Japan
Journal Title
British Ceram Trans 94 3 1995 109-111
Sector
Glass Ceramics
Class
GC 208