Oxy-Fuel Conversion Reduces Fuel Consumption For Glassfibre Melting

In recent years, oxy-fuel combustion has become widely embraced for the many benefits it brings to glass melting operations. In this article, the authors review a full furnace conversion accomplished at a furnace rebuild at Fiber Glass Industries (FGI), USA.

Author
J Rossi Et Al
Origin
Fiber Glass Inc, Usa
Journal Title
Glass Worldwide July-Aug/2011 45-48
Sector
Glass Fibre
Class
GF 627b