The vast majority of decorating techniques are described in this article, including screen printing, spray decorating, pad printing, labelling and decal decorating.
Origin
Kammann Machines Inc, New York, Usa
Journal Title
Glass 69 7 1992 263-264
Sector
General
Class
G 792