The ability of probe cation's to detect mixed coordination spheres is examined with reference to the implications for borate-fluoride glasses.
Origin
Unknown
Journal Title
Physics And Chemistry Of Glasses 1982 23 (2) 53-57
Sector
Primary Papers
Class