The relationships between host glass composition and optical properties of rare earth ions were studied by means of absorption and emission spectroscopy.
Origin
Otto-Schott-Inst, Jena, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 10 1998 289-299
Sector
Special Glass
Class
S 1568