Nucleation rates were measured in a ZrF4-BaF2-NaF-LaF3-AlF3 glass using an optical technique and the results compared with a similar glass with a slightly different composition.
Origin
Eindhoven University Of Technology
Journal Title
J Am Ceram Soc 1989 72 10 1991-1992
Sector
Glass Fibre
Class
GF 47