Post-HIPed pressureless sintered boron carbide not only yields lighter-weight armour but also enables forming of complex shapes for personal and vehicle armour.
Origin
Georgia Inst Technology & Verco Materials, Usa
Journal Title
Am Ceram Soc Bull 85 3 2006 21-23
Sector
Special Glass
Class
S 3109