A novel lift-out roll made from a modified heat resistant steel has been used for more than four years trouble free operation on a float glass line at the Asahi Glass Company LTD.
Origin
Unknown
Journal Title
Glastechnische Berichte 1983 56K (1) 265-270
Sector
Primary Papers
Class
PP 391