A dispersion-flattened single-mode fibre has been manufactured which has chromatic dispersion zeros at both 1.3 and 1.55 micrometre wavelengths.
Origin
Schott Glaswerke
Journal Title
Glastech Ber 1989 62 2 52-55
Sector
Glass Fibre
Class
GF 32