(100-x)B203xLi20 (mol%) glasses with x=0-50 were prepared by conventional melting technique and exposed to y-ray radiation. The CW-EPR spectra were recorded at room temperature and show a strong dependence on x. Echo induced EPR spectrum of the B203 glass is different from the CW-EPR spectrum showing better resolution. The FID spectrum of this centre contains valuable information about the structure of this centre.
Origin
Inst Mat Sci, Paraskevi Attikis, Greece
Journal Title
Phys Chem Glasses 38 1 1997 21-24