The suitability of fibre reinforcement of ceramic materials in engineering, including the fabrication of uni-, bi- and multi-directional reinforced composites, is discussed with particular emphasis on sol-gel procedures to provide matrices.
Origin
Gec Engineering Research Centre
Journal Title
Ceramic Industries International June 1989 32, 35-36, 38
Sector
Glass Fibre
Class
GF 36