Monazite was continuously coated onto Nextel 720 fibres, using an aqueous precursor and in-line heat treatment at 900-1300 deg C. Some experiments were repeated with alumina-doped precursors. Coated fibres were heat-treated for 100h at 1200 deg C. Coatings were characterized by optical microscopy, scanning electron microscopy, and analytical transmission electron microscopy. Coated-fibre tensile strengths were measured by single-filament tensile tests. The precursors were characterized by X-ray diffractometry, differential thermal analysis/thermogravimetric analysis, and mass spectrometry.
Origin
Wirght-Patterson Air Force Base, Usa
Journal Title
J Am Ceram Soc 84 12 2001 2783-2792
Sector
Glass Fibre
Class
GF 304