The behaviour of the Vogel-Fulcher-Tammann (VFT), MYEGA functions of viscous flow in relation to t = Tgl(T-To) is analysed, where Tg is glass transition temperature and To is the temperature in the VFT equation at which the configurational entropy becomes zero.