This article describes the challenges associated with using computational simulations to analyse and optimise an industrial furnace's performance, and a collaborative research effort that sought to improve common reaction models.
Origin
Unknown
Journal Title
Glass International March 2017 74-76
Sector
General
Class
G 4566