Density, refractive index, and infrared spectra were measured for calcium alumino-galliosilicate glasses containing 30 mol% CaO. The glasses exhibited additive behaviour in all properties.
Origin
Alfred University
Journal Title
J Am Ceram Soc 1989 72 9 1751-1754
Sector
Special Glass
Class
S 324