Transparent bulk Co2+:ZnAl2O4/SiO2 nanocomposites containing nanocrystalline Co2+:ZnAl2O4 dispersed in silica glass matrix were obtained by the sol-gel method.
Origin
Shandong University, China
Journal Title
Jacs 88 2 2005 399-403
Sector
Special Glass
Class
S 3006