SEM, TEM & HREM have been used to study microstructural characteristics of oxide-nonoxide composites; commonly found microcracks led to improved thermal shock resistance.
Origin
Univ Sci & Technol, Beijing, China
Journal Title
Am Ceram Soc Bull 79 2 February 2000
Sector
Refractories
Class
R 348