Melting Reactions In A Granulated Na2O-Cao-Sio2 Glass Batch Studied By Xrd And Mass Spectroscopy

The effects of granulation by spray drying and tumbling ont he glass batch reactions and homogeneity of the melted glass were investigated for a Na2O-CaO-SiO2 system. Primary materials with a wide range of sizes were employed. The melting temperature of the mixture decreased when slurrying was carried out using fine (average particle size (D50)

Author
T Tsujimura Et Al
Origin
Asahi Glass Co, Japan
Journal Title
Glass Technol Eur J Glass Sci 53 5 2012 202-210
Sector
Special Glass
Class
S 3944