Melting Behaviour Of Glasses In The Sr0-Mg0-Zr02-Si02 System

In the Sr0-Mg0-Zr02-Si02 system, a large range of compositions with 60, 55, 50, 45, 40, and 35 wt% silica has been thoroughly investiagted. The effect of silica and other constituents on melting, annealing and colour variations are reported in this paper.

Author
B Karasu
Origin
Anadolu University, Turkey
Journal Title
Glass Technology 40 3 1999 92-96