This paper describes a method of measurement and control of coloured glass. The examples of measurement of colour, dominant wavelength, colour purity, and colour brightness as well as control of colour are given by means of CIE 1964, and also the control range of colour in the glass is presented.
Origin
Henan Zhenghua Glass Process Factory, Shangqui, China
Journal Title
Proc Xvii Int Cong Glass, Vol 7, Beijing 1995, 125-128
Sector
Special Glass
Class
S 1393