The Market For Ferrules Is Booming

The global fibre optic technology market is booming. This paper describes ARBURG's ceramic injection moulding system for the production of ferrules, which are the plugs linking fibre optic cables used in modern data transfer systems. The system allows everything from feedstock to production lines to be provided by a single supplier.

Author
H Walcher
Origin
Arburg Gmbh, Germany
Journal Title
International Ceramics 2 2001 19, 21-22
Sector