In this article the authors consider how to improve the efficiency and profitability of bushing positions by smart design of the entire system, from the incoming power to the precious metal.
Origin
Unknown
Journal Title
Glass Worldwide Nov-Dec 2012 58-61
Sector
Glass Fibre
Class
GF 660