Machining Of Interpenetrating Phase Alumina/Aluminium Composite By Electrical Discharge Technique

Factors influencing the behaviour of alumina/aluminium inter penetrating phase composite during wire-cut electrical discharge machining (WEDM) are studied. Machining performance in terms of material removal rate and surface roughness were compared under different machining conditions. Results show that the matching process affects the surface quality of the machined composite.

Author
S K Roy Et Al
Origin
Cgcri, India
Journal Title
Trans Ind Ceram Soc 67 2 2008 75-80