Local Structure, Valence States And Magnetic Interactions Of Copper Ions In A 2B203.Te02 Glass Matrix

Glasses from xCuO.(100-x)[2B2O3.TeO2] system with O4 mol% of Cu2+ and Cu+ species. The Curie behaviour of magnetic susceptibility indicates the presence of isolated and/or dipole-dipole coupled interactions of Cu2+ ions.