The local environment of transition metal (M) and lead has been studied for Mt11=Mn2+, Zn2+; Mt1111=Fe3+, Ga3+. Theoretical phase shifts and backscatter amplitude are used after testing with crystallised fluorides of various structures.
Origin
Unknown
Journal Title
J. Solid St Chem., 1984, 52 (1), 32-44 (French)
Sector
Primary Papers
Class
PP 800