The factors involved in the nucleation and crystallisation of lithium aluminosilicate glass ceramics and the properties of the resultant materials are reviewed. Applications, including oven top panels, telescopes and lasers, are also described.
Origin
Schott Glaswerke
Journal Title
Ceramic Bulletin 1989 68 11 1926-1930
Sector
Glass Ceramics
Class
GC 59