Perhaps the greatest challenge to date in the ceramic industry is the immediate requirement to further reduce lead release levels from lead-containing glazes and decorations used on the food contact surface of ceramic ware, to within new US Food & Drug Adminstrations limits and to comply with California's Safe Drinking Water & Toxic Enforcement Act of 1986.