Lcd Substrate - The Future Process

In the last two years the production of LCD substrate glass has again reached a high technological level. This has been achieved with a now well-known process called the Overflow Down Draw Process (ODDP). The contribution of EGLASSTREK, with 40 years of experience in the domain of direct-fired platinum tubes, together with a renowned German equipment supplier, has led to the construction of turnkey sheet glass-manufacturing installations featuring the ODDP.

Author
D Bottger
Origin
Eglasstrek Gmbh, Germany
Journal Title
Int Glass Review 2/2000 20-22