Following the first part of this article where the properties of glass for laser fusion applications were examined, this second part gives a brief overview of laser glass technology evolution. Also discussed are developments in manufacturing, with particular emphasis on improved laser damage threshold, edge cladding development and advances in melting technology.
Origin
Lawrence Livermore National Labs, Usa
Journal Title
Gmpa 5/99 129-137
Sector
Special Glass
Class
S 1751