The influence of the two polyvalent ions, cobalt and nickel, on the formation of irradiation-induced defects was studied in several different model glasses (silicate, borosilicate, fluoride and phosphate glasses). In this article the defects are demonstrated on the example of the (SrPO3)2-metaphosphate glass P100.
Origin
Otto-Schott Inst, Germany
Journal Title
Glastech Ber Glass Sci Technol 74 7 2001 199-209
Sector
Special Glass
Class
S 2242