Recent progress in the production of integrated optical components by ion exchange in glass for applications such as sensor or communication techniques is reviewed.
Origin
Ict Entwicklungsgesellschaft Fur Integrierte Optik-Technologie Gmbh
Journal Title
Glastech Ber 1989 62 8 285-297
Sector
Special Glass
Class
S 318