This paper describes results from a mathematical modelling based study of fluid flow and heat transfer phenomena in the melting and delivery ends of an oxy-fuel glass furnace. The three-dimensional mathematical model used in this study not only integrates phenomena taking place in the various sub-domains of the two sections, it also integrates the two sections themselves.
Origin
Owens-Corning, Usa
Journal Title
Proc Icg Vol 2 Extended Abstracts 2001 364
Sector
Special Glass
Class
S 2755