Initial Stages Of Glass Corrosion In Water

A surface analytical study has been made of a soda-lime-silica glass treated for 15, 30, 60 and 120 minutes in normal and isotopically labelled water.

Author
T Richter Et Al
Origin
Techn Univ Clausthal, Ecole National Superieure Des Mines De Nancy
Journal Title
Glastech Ber 1990 63 10 300-308