Infrared Spectra Of Hydrogen Bonded Hydroxyl Groups In Silicate Glasses. A Reinterpretation

Infrared spectra of water containing alkali silicate and similar glasses in the region of OH stretching vitrations are reconsidered in a general context of vitrational spectroscopy of hydrogen bonded systems.

Author
D P Zarubin
Origin
Food Industry Institute, Russia
Journal Title
Phys Chem Glasses 40 4 1999 184-192
Sector
Special Glass
Class
S 1739

Request article (free for British Glass members)

Infrared Spectra Of Hydrogen Bonded Hydroxyl Groups In Silicate Glasses. A Reinterpretation
Phys Chem Glasses 40 4 1999 184-192
S 1739